The following is a range of improved properties in alloy steels:-
In order to improve some of these above mentioned properties, the material should go through the process of heat treatment. Our company has following grades in stock.
This grade should be heated slowly to 860-890°C and after adequate soaking at this temperature, quench in oil. Temper as soon as tools reach room temperature. Tempering should be done at 480-595°C. Soak at the temperature for 2 hours per 25mm of ruling section, and then allow cooling in air. Tempering between 250-375°C is not advised as tempering within this range will reduce the impact value.
Treatment | Condition | Temperature cycle | Cooling/quenching |
---|---|---|---|
Soft annealing | +A | 670 - 710°C | In air |
Quench & Tempering | +QT |
Austenizing 830 - 860°C Tempering 540 - 680°C |
Water or oil |
Grade | Quenching Temperature, ºC | Hardness | 150ºC | 200ºC | 300ºC | 400ºC | 500ºC | 550ºC | 600ºC | 650ºC |
---|---|---|---|---|---|---|---|---|---|---|
51CrV4 | 860ºC | 56-62 | 56 | 55 | 51 | 45 | 39 | 35 | 31 | 28 |
Location 1:- 53-D, Haji Park, Bundh Road, Lahore-Pakistan
Location 2:- Service Road, Ring Road, Near Sialkot-Lahore Motorway Bridge, Lakhodair, Lahore-Pakistan
Location 1:- 53-D, Haji Park, Bundh Road, Lahore Pakistan
Location 2:- Service Road, Ring Road, Near Sialkot-Lahore Motorway Bridge, Lakhodair, Lahore-Pakistan
+923008448470 +923314367768 +971566093063
info@mmturbo.com euro.steel642@hotmail.com altaf54@hotmail.com
WhatsApp us